Very nice. So that was the CC soft with 1/4 cup salt per 8 oz plastic. No other softener was added? It looked pretty soft still. How is durability?
Thanks...Bill
That was done in March - it could have been an early formula of CC or MF. Either way I'm sure it had softener in it. I did that on the fly and was mainly focused the salt / plastic ratio.