Hey There-
I am having trouble with denting on the left side of the bait. The dent is the same every time. I have been able to produce some baits without dents but certainly more with than without. I can't seem to figure out the step I am missing. Here are some details:
Plastic: CC Soft
Mold: CC 4.5 Swim Shad
Plastic Temp: Around 350
Color: None, Pearl, Green Pumpkin
Glitter: Silver, Red or Black Flake
Injector: CC 4 oz
Heating Method: Microwave
Injecting steps: Draw plastic, "burp the injector to get out the air, insert injector to mold, hold for 3 secs, inject slowly, hold for 5 secs after feeling back pressure, continue to fill the sprue as it draws down
Clamps: 3 600 lb Irwin front middle and rear
Problem area: left side (looking from front to back) - upper side as it sits in the mold - the dent is on the body just behind the nose but not affecting the tail - no major air bubbles to speak of