I gave it another whirl.I'd like to thank some good customer service.If you're doing laminates the mold shoots best between 85-90 degrees. I'm getting clean laminates better than I was before.When doing them the same general rules for laminates/twinjecting still apply.I shot a few single color & only had 1 fail but the one that failed was because of my own doing as I tried to shoot it too cool. I will have a vid up by sat/sunday as some requested .